Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Orgalloy® LT 4060 ES BLACK T6L - PA6... - ARKEMA

Material Data Center offers the following functions for Orgalloy® LT 4060 ES BLACK T6L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Orgalloy LT datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Orgalloy® LT 4060 ES BLACK T6L resin is a polyamide alloy especially designed for extrusion blow molding. This black grade offers an excellent thermal resistance, cold impact performance and flexibility.

Main applications:
  • Automotive air intake ducts (clean air duct and outside intercooler tube)


Packaging:
This grade is delivered dried in sealed packaging (25kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 0.5 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 5 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 570 / 230 MPa ISO 527
Stress at 50% strain 22 / 16 MPa ISO 527
Strain at break >50 / >50 % ISO 527
Charpy notched impact strength, +23°C 79 / 78 kJ/m² ISO 179/1eA
Shore D hardness 50 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 220 / * °C ISO 11357-1/-3
Temp. of deflection under load, 0.45 MPa 60 / * °C ISO 75-1/-2
Vicat softening temperature, B 62 / * °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 5 / * % Sim. to ISO 62
Humidity absorption 1.1 / * % Sim. to ISO 62
Density 1040 / 1040 kg/m³ ISO 1183
Diagrams
Specific volume-temperature (pvT) , Orgalloy® LT 4060 ES BLACK T6L, PA6..., ARKEMA
Characteristics
Processing
Blow Molding
Delivery form
Pellets, Black
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Blow molding
Processing conditions:
- Drying time (only necessary for bags opened for more than two hours): 4-8 hours at 80°C
- Extrusion melt temperature (min-recommended-max): 250-260-270°C 
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.